Saleh, B., Alkanhal, T., Ahmed, S. (2013). FRACTAL CHARACTERIZATION OF CAVITATION DAMAGE OF CARBURIZED AISI 5117 STEE. JES. Journal of Engineering Sciences, 41(No 2), 517-542. doi: 10.21608/jesaun.2013.114747
B. Saleh; Tawfeeq A. Alkanhal; S. M. Ahmed. "FRACTAL CHARACTERIZATION OF CAVITATION DAMAGE OF CARBURIZED AISI 5117 STEE". JES. Journal of Engineering Sciences, 41, No 2, 2013, 517-542. doi: 10.21608/jesaun.2013.114747
Saleh, B., Alkanhal, T., Ahmed, S. (2013). 'FRACTAL CHARACTERIZATION OF CAVITATION DAMAGE OF CARBURIZED AISI 5117 STEE', JES. Journal of Engineering Sciences, 41(No 2), pp. 517-542. doi: 10.21608/jesaun.2013.114747
Saleh, B., Alkanhal, T., Ahmed, S. FRACTAL CHARACTERIZATION OF CAVITATION DAMAGE OF CARBURIZED AISI 5117 STEE. JES. Journal of Engineering Sciences, 2013; 41(No 2): 517-542. doi: 10.21608/jesaun.2013.114747
FRACTAL CHARACTERIZATION OF CAVITATION DAMAGE OF CARBURIZED AISI 5117 STEE
1Mechanical Eng Department, Faculty of Engineering, Assiut University, Assiut, Egypt
2Research Center director of Engineering and Applied Science, Faculty of Engineering, Majmaah University, Saudi Arabia
3Mechanical Engineering Department, Faculty of Engineering, Majmaah University ,Saudi Arabia
Abstract
The cavitation erosion of carburized and untreated low alloy steel (AISI 5117) has been investigated during the incubation period. Scanning electron microscope images of eroded surface were obtained, forming a data base for further analysis. It has been shown that carburizing can effectively improve the cavitation erosion resistance of AISI 5117 low alloy steel and prolong the incubation period. The fractal dimension and Fourier intercept values can be used to characterize the cavitation damage. The fractal dimension and Fourier intercept value for the untreated surfaces were higher than that of the carburized surfaces.